International Atlas of Casting Defects
Download or Read eBook International Atlas of Casting Defects PDF written by Mervin T. Rowley and published by Amer Foundry Society. This book was released on 1974-01-01 with total page 337 pages. Available in PDF, EPUB and Kindle.
Author | : Mervin T. Rowley |
Publisher | : Amer Foundry Society |
Total Pages | : 337 |
Release | : 1974-01-01 |
ISBN-10 | : 087433053X |
ISBN-13 | : 9780874330533 |
Rating | : 4/5 (3X Downloads) |
Book Synopsis International Atlas of Casting Defects by : Mervin T. Rowley
Book excerpt: The object of this book is to assist in maintaining a constant increase in the quality of castings. To achieve this it is necessary to facilitate the suppression of defects. This book attempts to do by making defects better known or recognized, by indicating possible causes, and by recommending suitable measures for their elimination.